Investigation determined that internal galling has caused the failure rendering the needle valve unusable. The galling was caused by a stainless steel stem acting against a stainless steel seat. This failure mode had been observed before and the…
High-pressure fueling hoses should be examined daily for signs of external damage, including corrosion, abrasion, cuts, and kinking. High-use fueling hoses should be replaced every six months.